• Quenched and Tempered Alloy Steel.
• Manufactured in accordance with EN 1677- 3.
• Manufactured in accordance with ASTM A952/A952M, DIN PAS 1061.
• Proof Load tested at 2.5 times the WLL with certification for each batch manufactured.
• Design Factor 4:1.
• Fatigue rated to 20,000 cycles at 1.5 times the WLL.
• Tempering temperature minimum 400°C
• Magnaflux crack detection is performed 100% on each batch.